The authors compared the tensile bond strength of a self-etching primer system to enamel and dentin prepared with a bur, Er:YAG laser, or Er,Cr:YSGG laser. Bond strength was higher on Er:YAG-treated surfaces than on Er,Cr:YSGG-treated surfaces, but both laser groups were lower than the bur-cut control. The study used 30 enamel and 30 dentin samples divided into three groups each.
- Who or what was studied
- Enamel and dentin samples from teeth (30 of each substrate, divided into three groups)
- Limits stated in the abstract
- The abstract reports only a laboratory tensile bond strength test on a small number of samples, without clinical outcomes.
Written by an AI model from this paper’s abstract only and checked automatically against it, but it can still be wrong. It is not medical advice. Read the full paper. See the editorial policy.
Abstract
The full abstract is not shown here because it is protected by the publisher’s copyright. Read it on journals.sagepub.com.
Record from PubMed, a service of the National Library of Medicine.
How to read a single study: what to check before relying on this kind of research.
Terms in this paper: Laser. Each links to its definition in the glossary.
A summary of published research, not medical advice. One study rarely settles a question. See the disclaimer and how to read research.