Resumen generado por IA
Este estudio in vitro comparó tratamientos superficiales para postes de fibra de vidrio (peróxido de hidrógeno, láser de fibra de iterbio y terapia láser de baja intensidad mediada por ftalocianina) y su efecto sobre la rugosidad superficial, la resistencia a la flexión y la resistencia de unión a la dentina radicular. Los autores informan de que el peróxido de hidrógeno produjo la mayor rugosidad y la menor resistencia a la flexión, mientras que los postes sin tratar tuvieron la menor rugosidad y la mayor resistencia a la flexión. También informan de que el láser de fibra de iterbio dio resultados satisfactorios y que el cemento autoadhesivo superó al cemento convencional.
- Participantes
- 80
- Quién o qué se estudió
- Ochenta dientes premolares inferiores monorradiculares, con 120 postes de fibra de vidrio asignados a cuatro grupos de acondicionamiento.
- Límites indicados en el resumen
- El estudio es in vitro, utiliza dientes y postes extraídos en lugar de pacientes vivos, por lo que no se puede inferir el rendimiento clínico.
Traducido por un modelo de IA a partir del resumen en inglés, que se escribió solo a partir del resumen de este artículo. Las cifras se comprobaron automáticamente con el resumen del artículo, pero el texto aun así puede ser incorrecto. No es consejo médico. Lee el artículo completo. Consulta la política editorial.
Resumen (abstract)
Objective
Assessing the impact of different surface conditioners (Hydrogen peroxide (H2O2), Ytterbium fiber laser (YFL), Low-level laser therapy (LLLT)-Phthalocyanine (Pc) on the surface characterization, flexural strength (FS), surface roughness (Ra) and push-out bond strength (POBS) of glass fiber post (GFP) bonded to root dentin using conventional resin cement (CRC) and self-adhesive resin cement (SARC). METHODOLOGY: This in-vitro study included eighty single-rooted mandibular premolar teeth, and subsequently, crowns were decoronated. Ethical approval was obtained from Dar Al Uloom University (COD/IRB/2025/91; Dated February 15, 2025). The study duration was six months. 120 GFP were allocated to four groups according to the conditioning protocol. Group-1 (No conditioning), Group-2 (H2O2), Group-3 (YFL), and Group-4 (1% Pc-LLLT). Scanning Electron Microscopy (SEM) was performed to assess the surface topography. Ra was measured using a profilometer. The three-point bending test was used to evaluate the flexural strength (FS). Root canal procedure was performed, followed by post space preparation. Twenty GFPs were distributed into two subgroups based on the bonding technique- Subgroup A: CRC via total etch (TE); Subgroup B: SARC.POBS and bond failure assessment were performed using a universal testing machine and a stereomicroscope. Two-way ANOVA and Tukey post hoc test were applied for all comparisons.
Results
The highest Ra and lowest FS were seen in Group-2 (H2O2). The lowest Ra and the highest FS were observed in Group-1 (No conditioning) samples. The highest POBS was observed in the cervical third of Group-2A (H2O2+CRC). Conversely, the lowest bond strengths were observed in the apical section of Group-4A (1% Pc-LLLT+CRC).
Conclusion
The yttrium fiber laser demonstrated satisfactory Ra, FS, and POBS for the glass fiber post. Self-adhesive resin cement outperformed conventional luting cement.
Resumen reproducido bajo la licencia CC BY. Fuente: PubMed, un servicio de la National Library of Medicine.
Cómo leer un estudio individual: qué comprobar antes de fiarte de este tipo de investigación.
Términos de este artículo: Terapia láser de baja intensidad, Láser. Cada uno enlaza con su definición en el glosario.
Un resumen de investigación publicada, no consejo médico. Un solo estudio rara vez resuelve una cuestión. Consulta el aviso legal y cómo leer la investigación.